SAE International Etch Inspection of High Strength Steel Parts AMS2649C

Description
This specification establishes the requirements for etch inspection of bare high-strength low-alloy steel parts having tensile strength of 180 ksi (1241 MPa) and higher and of carburized parts to detect overheating caused by abusive machining or grinding in the heat treated condition, and to detect localized discontinuous carburization. This process is not applicable to surface hardened steels produced by nitriding or carbonitriding. This process may remove 0.0001 to 0.0005 inch (2.5 to 12.7 micrometers) from the surface of the part.
Description
This specification establishes the requirements for etch inspection of bare high-strength low-alloy steel parts having tensile strength of 180 ksi (1241 MPa) and higher and of carburized parts to detect overheating caused by abusive machining or grinding in the heat treated condition, and to detect localized discontinuous carburization. This process is not applicable to surface hardened steels produced by nitriding or carbonitriding. This process may remove 0.0001 to 0.0005 inch (2.5 to 12.7 micrometers) from the surface of the part.

Suppliers

Company
Product
Description
Supplier Links
Etch Inspection of High Strength Steel Parts - AMS2649C - SAE International
Warrendale, PA, United States
Etch Inspection of High Strength Steel Parts
AMS2649C
Etch Inspection of High Strength Steel Parts AMS2649C
This specification establishes the requirements for etch inspection of bare high-strength low-alloy steel parts having tensile strength of 180 ksi (1241 MPa) and higher and of carburized parts to detect overheating caused by abusive machining or grinding in the heat treated condition, and to detect localized discontinuous carburization. This process is not applicable to surface hardened steels produced by nitriding or carbonitriding. This process may remove 0.0001 to 0.0005 inch (2.5 to 12.7 micrometers) from the surface of the part.

This specification establishes the requirements for etch inspection of bare high-strength low-alloy steel parts having tensile strength of 180 ksi (1241 MPa) and higher and of carburized parts to detect overheating caused by abusive machining or grinding in the heat treated condition, and to detect localized discontinuous carburization. This process is not applicable to surface hardened steels produced by nitriding or carbonitriding. This process may remove 0.0001 to 0.0005 inch (2.5 to 12.7 micrometers) from the surface of the part.

Supplier's Site

Technical Specifications

  SAE International
Product Category Standards and Technical Documents
Product Number AMS2649C
Product Name Etch Inspection of High Strength Steel Parts
Unlock Full Specs
to access all available technical data

Similar Products