Applications / Materials Joined
Root and Hot Pass Welding of up to X80 Grade Pipe, When Followed by Low Hydrogen Fill and Cap, API 5L X70 Through X80 Grade Pipe, Cross Country Pipe
Joining Process / Product Form
Stick (SMAW) Electrode
Diameter / Thickness
0.1250 to 0.1875 inch (3.17 to 4.76 mm)
Joining Process / Product Form
Braze or solder in the form of a paste. (optional feature); Powder (optional feature); Strip, sheet or foil (optional feature); Solid wire or rod (optional feature)