Accuris NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH AMS5582

Description
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH
Request a Quote
Description
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH
Request a Quote

Suppliers

Company
Product
Description
Supplier Links
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH - AMS5582 - Accuris
Englewood, CO, United States
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH
AMS5582
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH AMS5582
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH

NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH

Buy Now

Technical Specifications

  Accuris
Product Category Standards and Technical Documents
Product Number AMS5582
Product Name NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB (NB) - 2.5TI - 0.70AL - 7.0FE SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH
Unlock Full Specs