CSA Group Rubber, vulcanized or thermoplastic - Determination of compression set - Part 2: At low temperatures ISO 815-2:2014

Description
ISO 815-2:2014 specifies two methods for the determination of the compression set characteristics of vulcanized and thermoplastic rubbers at low temperatures. Method 1 derives from the methodology used in ISO 815‑1. Method 2 uses a specified testing device, allowing to measure and record the test piece thickness during recovery. Due to the load applied during recovery in method 2, no correlation can be established between the results given by both methods.
Description
ISO 815-2:2014 specifies two methods for the determination of the compression set characteristics of vulcanized and thermoplastic rubbers at low temperatures. Method 1 derives from the methodology used in ISO 815‑1. Method 2 uses a specified testing device, allowing to measure and record the test piece thickness during recovery. Due to the load applied during recovery in method 2, no correlation can be established between the results given by both methods.

Suppliers

Company
Product
Description
Supplier Links
Rubber, vulcanized or thermoplastic - Determination of compression set - Part 2: At low temperatures - ISO 815-2:2014 - CSA Group
Toronto, Ontario, Canada
Rubber, vulcanized or thermoplastic - Determination of compression set - Part 2: At low temperatures
ISO 815-2:2014
Rubber, vulcanized or thermoplastic - Determination of compression set - Part 2: At low temperatures ISO 815-2:2014
ISO 815-2:2014 specifies two methods for the determination of the compression set characteristics of vulcanized and thermoplastic rubbers at low temperatures. Method 1 derives from the methodology used in ISO 815‑1. Method 2 uses a specified testing device, allowing to measure and record the test piece thickness during recovery. Due to the load applied during recovery in method 2, no correlation can be established between the results given by both methods.

ISO 815-2:2014 specifies two methods for the determination of the compression set characteristics of vulcanized and thermoplastic rubbers at low temperatures.

Method 1 derives from the methodology used in ISO 815‑1. Method 2 uses a specified testing device, allowing to measure and record the test piece thickness during recovery. Due to the load applied during recovery in method 2, no correlation can be established between the results given by both methods.

Supplier's Site

Technical Specifications

  CSA Group
Product Category Standards and Technical Documents
Product Number ISO 815-2:2014
Product Name Rubber, vulcanized or thermoplastic - Determination of compression set - Part 2: At low temperatures
Unlock Full Specs
to access all available technical data

Similar Products