ISO 7146-2:2008 defines, describes and classifies the characteristics of damage occurring in service in hydrodynamically lubricated metallic plain bearings due to cavitation erosion, together with possible countermeasures. It assists in understanding the various characteristic forms of damage which may occur. Consideration is restricted to damage which has a well-defined appearance and which can be attributed to particular causes with a high degree of certainty. Various appearances are illustrated with photographs and diagrams.
Description
ISO 7146-2:2008 defines, describes and classifies the characteristics of damage occurring in service in hydrodynamically lubricated metallic plain bearings due to cavitation erosion, together with possible countermeasures. It assists in understanding the various characteristic forms of damage which may occur. Consideration is restricted to damage which has a well-defined appearance and which can be attributed to particular causes with a high degree of certainty. Various appearances are illustrated with photographs and diagrams.

Suppliers

Company
Product
Description
Supplier Links
Plain bearings - Appearance and characterization of damage to metallic hydrodynamic bearings - Part 2: Cavitation erosion and its countermeasures - ISO 7146-2:2008 - CSA Group
Toronto, Ontario, Canada
Plain bearings - Appearance and characterization of damage to metallic hydrodynamic bearings - Part 2: Cavitation erosion and its countermeasures
ISO 7146-2:2008
Plain bearings - Appearance and characterization of damage to metallic hydrodynamic bearings - Part 2: Cavitation erosion and its countermeasures ISO 7146-2:2008
ISO 7146-2:2008 defines, describes and classifies the characteristics of damage occurring in service in hydrodynamically lubricated metallic plain bearings due to cavitation erosion, together with possible countermeasures. It assists in understanding the various characteristic forms of damage which may occur. Consideration is restricted to damage which has a well-defined appearance and which can be attributed to particular causes with a high degree of certainty. Various appearances are illustrated with photographs and diagrams.

ISO 7146-2:2008 defines, describes and classifies the characteristics of damage occurring in service in hydrodynamically lubricated metallic plain bearings due to cavitation erosion, together with possible countermeasures. It assists in understanding the various characteristic forms of damage which may occur.

Consideration is restricted to damage which has a well-defined appearance and which can be attributed to particular causes with a high degree of certainty. Various appearances are illustrated with photographs and diagrams.

Supplier's Site

Technical Specifications

  CSA Group
Product Category Standards and Technical Documents
Product Number ISO 7146-2:2008
Product Name Plain bearings - Appearance and characterization of damage to metallic hydrodynamic bearings - Part 2: Cavitation erosion and its countermeasures
Unlock Full Specs
to access all available technical data

Similar Products