CSA Group Plastics - Unsaturated polyester resins - Determination of reactivity at 80 degrees C (conventional method) ISO 584:1982

Description
Specifies a method for the determination of the reactivity of unsaturated polyester resins as characterized by the maximum temperature reached when heated with catalyst in a water-bath at 80 °C and by the time taken for the temperatur of the mixture to rise from 65 °C to this maximum temperature. As the test results depend very much on the conditions under which the test is carried out, these conditions are described in detail.
Description
Specifies a method for the determination of the reactivity of unsaturated polyester resins as characterized by the maximum temperature reached when heated with catalyst in a water-bath at 80 °C and by the time taken for the temperatur of the mixture to rise from 65 °C to this maximum temperature. As the test results depend very much on the conditions under which the test is carried out, these conditions are described in detail.

Suppliers

Company
Product
Description
Supplier Links
Plastics - Unsaturated polyester resins - Determination of reactivity at 80 degrees C (conventional method) - ISO 584:1982 - CSA Group
Toronto, Ontario, Canada
Plastics - Unsaturated polyester resins - Determination of reactivity at 80 degrees C (conventional method)
ISO 584:1982
Plastics - Unsaturated polyester resins - Determination of reactivity at 80 degrees C (conventional method) ISO 584:1982
Specifies a method for the determination of the reactivity of unsaturated polyester resins as characterized by the maximum temperature reached when heated with catalyst in a water-bath at 80 °C and by the time taken for the temperatur of the mixture to rise from 65 °C to this maximum temperature. As the test results depend very much on the conditions under which the test is carried out, these conditions are described in detail.

Specifies a method for the determination of the reactivity of unsaturated polyester resins as characterized by the maximum temperature reached when heated with catalyst in a water-bath at 80 °C and by the time taken for the temperatur of the mixture to rise from 65 °C to this maximum temperature. As the test results depend very much on the conditions under which the test is carried out, these conditions are described in detail.

Supplier's Site

Technical Specifications

  CSA Group
Product Category Standards and Technical Documents
Product Number ISO 584:1982
Product Name Plastics - Unsaturated polyester resins - Determination of reactivity at 80 degrees C (conventional method)
Unlock Full Specs
to access all available technical data

Similar Products