CSA Group Plastics - Polypropylene and propylene-copolymers - Determination of thermal oxidative stability in air - Oven method ISO 4577:1983

Description
Specifies a method for the determination of the resistance of moulded test specimens of propylene and propylene-copolymers to acclerated ageing at specified temperatures in the range from 100 to 150oC in a forced draught oven. Rotating specimen holders are recommended.- The time to failure is determined by visual examination and taken as the number of days after which a specimen shows localized crazing, crumbling and/or discoloration. The test may be conducted at several temperatures and the data interpreted by the use of the Arrhenius relation.
Description
Specifies a method for the determination of the resistance of moulded test specimens of propylene and propylene-copolymers to acclerated ageing at specified temperatures in the range from 100 to 150oC in a forced draught oven. Rotating specimen holders are recommended.- The time to failure is determined by visual examination and taken as the number of days after which a specimen shows localized crazing, crumbling and/or discoloration. The test may be conducted at several temperatures and the data interpreted by the use of the Arrhenius relation.

Suppliers

Company
Product
Description
Supplier Links
Plastics - Polypropylene and propylene-copolymers - Determination of thermal oxidative stability in air - Oven method - ISO 4577:1983 - CSA Group
Toronto, Ontario, Canada
Plastics - Polypropylene and propylene-copolymers - Determination of thermal oxidative stability in air - Oven method
ISO 4577:1983
Plastics - Polypropylene and propylene-copolymers - Determination of thermal oxidative stability in air - Oven method ISO 4577:1983
Specifies a method for the determination of the resistance of moulded test specimens of propylene and propylene-copolymers to acclerated ageing at specified temperatures in the range from 100 to 150oC in a forced draught oven. Rotating specimen holders are recommended.- The time to failure is determined by visual examination and taken as the number of days after which a specimen shows localized crazing, crumbling and/or discoloration. The test may be conducted at several temperatures and the data interpreted by the use of the Arrhenius relation.

Specifies a method for the determination of the resistance of moulded test specimens of propylene and propylene-copolymers to acclerated ageing at specified temperatures in the range from 100 to 150oC in a forced draught oven. Rotating specimen holders are recommended.- The time to failure is determined by visual examination and taken as the number of days after which a specimen shows localized crazing, crumbling and/or discoloration. The test may be conducted at several temperatures and the data interpreted by the use of the Arrhenius relation.

Supplier's Site

Technical Specifications

  CSA Group
Product Category Standards and Technical Documents
Product Number ISO 4577:1983
Product Name Plastics - Polypropylene and propylene-copolymers - Determination of thermal oxidative stability in air - Oven method