CSA Group Rubber, vulcanized or thermoplastic - Determination of stress relaxation in compression - Part 2: Testing with temperature cycling ISO 3384-2:2012

Description
ISO 3384-2:2012 specifies two methods for determining the decrease in counterforce exerted by a test piece of vulcanized or thermoplastic rubber which has been compressed to a constant deformation and then undergoes temperature cycling. Method A: The temperature is cycled at intervals between a high temperature for ageing and a low temperature for checking the sealing force at this low temperature. Method B: The temperature is cycled continuously between a high temperature and a low temperature to introduce thermal stress in the test piece. The counterforce is determined by means of a continuous-measureme nt system.
Description
ISO 3384-2:2012 specifies two methods for determining the decrease in counterforce exerted by a test piece of vulcanized or thermoplastic rubber which has been compressed to a constant deformation and then undergoes temperature cycling. Method A: The temperature is cycled at intervals between a high temperature for ageing and a low temperature for checking the sealing force at this low temperature. Method B: The temperature is cycled continuously between a high temperature and a low temperature to introduce thermal stress in the test piece. The counterforce is determined by means of a continuous-measureme nt system.

Suppliers

Company
Product
Description
Supplier Links
Rubber, vulcanized or thermoplastic - Determination of stress relaxation in compression - Part 2: Testing with temperature cycling - ISO 3384-2:2012 - CSA Group
Toronto, Ontario, Canada
Rubber, vulcanized or thermoplastic - Determination of stress relaxation in compression - Part 2: Testing with temperature cycling
ISO 3384-2:2012
Rubber, vulcanized or thermoplastic - Determination of stress relaxation in compression - Part 2: Testing with temperature cycling ISO 3384-2:2012
ISO 3384-2:2012 specifies two methods for determining the decrease in counterforce exerted by a test piece of vulcanized or thermoplastic rubber which has been compressed to a constant deformation and then undergoes temperature cycling. Method A: The temperature is cycled at intervals between a high temperature for ageing and a low temperature for checking the sealing force at this low temperature. Method B: The temperature is cycled continuously between a high temperature and a low temperature to introduce thermal stress in the test piece. The counterforce is determined by means of a continuous-measureme nt system.

ISO 3384-2:2012 specifies two methods for determining the decrease in counterforce exerted by a test piece of vulcanized or thermoplastic rubber which has been compressed to a constant deformation and then undergoes temperature cycling.

Method A: The temperature is cycled at intervals between a high temperature for ageing and a low temperature for checking the sealing force at this low temperature.

Method B: The temperature is cycled continuously between a high temperature and a low temperature to introduce thermal stress in the test piece.

The counterforce is determined by means of a continuous-measurement system.

Supplier's Site

Technical Specifications

  CSA Group
Product Category Standards and Technical Documents
Product Number ISO 3384-2:2012
Product Name Rubber, vulcanized or thermoplastic - Determination of stress relaxation in compression - Part 2: Testing with temperature cycling
Unlock Full Specs
to access all available technical data

Similar Products