IEC 61249-2-39:2012 specifies requirements for properties of modified brominated epoxide woven E-glass laminated sheet of a thickness 0,05 mm up to 3,2 mm, of defined flammability (vertical burning test), copper-clad. The glass transition temperature is defined to be 170 °C minimum.
Description
IEC 61249-2-39:2012 specifies requirements for properties of modified brominated epoxide woven E-glass laminated sheet of a thickness 0,05 mm up to 3,2 mm, of defined flammability (vertical burning test), copper-clad. The glass transition temperature is defined to be 170 °C minimum.

Suppliers

Company
Product
Description
Supplier Links
Materials for printed boards and other interconnecting structures - Part 2-39: Reinforced base materials clad and unclad - High performance epoxide and non-epoxide, woven E-glass laminate sheets of... - IEC 61249-2-39:2012 - CSA Group
Toronto, Ontario, Canada
Materials for printed boards and other interconnecting structures - Part 2-39: Reinforced base materials clad and unclad - High performance epoxide and non-epoxide, woven E-glass laminate sheets of...
IEC 61249-2-39:2012
Materials for printed boards and other interconnecting structures - Part 2-39: Reinforced base materials clad and unclad - High performance epoxide and non-epoxide, woven E-glass laminate sheets of... IEC 61249-2-39:2012
IEC 61249-2-39:2012 specifies requirements for properties of modified brominated epoxide woven E-glass laminated sheet of a thickness 0,05 mm up to 3,2 mm, of defined flammability (vertical burning test), copper-clad. The glass transition temperature is defined to be 170 °C minimum.

IEC 61249-2-39:2012 specifies requirements for properties of modified brominated epoxide woven E-glass laminated sheet of a thickness 0,05 mm up to 3,2 mm, of defined flammability (vertical burning test), copper-clad. The glass transition temperature is defined to be 170 °C minimum.

Supplier's Site

Technical Specifications

  CSA Group
Product Category Standards and Technical Documents
Product Number IEC 61249-2-39:2012
Product Name Materials for printed boards and other interconnecting structures - Part 2-39: Reinforced base materials clad and unclad - High performance epoxide and non-epoxide, woven E-glass laminate sheets of...
Unlock Full Specs
to access all available technical data

Similar Products