Celanese Corporation CELSTRAN PP-GF50-03 826

Description
It is normally not necessary to dry CELSTRAN PP. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is required.
Description
It is normally not necessary to dry CELSTRAN PP. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is required.

Suppliers

Company
Product
Description
Supplier Links
CELSTRAN PP-GF50-03 - 826 - Celanese Corporation
Irving, TX, USA
CELSTRAN PP-GF50-03
826
CELSTRAN PP-GF50-03 826
It is normally not necessary to dry CELSTRAN PP. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is required.

It is normally not necessary to dry CELSTRAN PP. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is required.

Supplier's Site

Technical Specifications

  Celanese Corporation
Product Category Polymers and Plastic Resins
Product Number 826
Product Name CELSTRAN PP-GF50-03
Type MoldingCompound; Thermoplastic
Unlock Full Specs
to access all available technical data

Similar Products

Exact™ Plastomer Resins for Film Packaging - Exact™ 4151 Cast - ExxonMobil - Polyethylene Products
Specs
Type FilmGrade; Thermoplastic
Tensile (Break) 11000 psi (75843 KPa)
Elongation 360.0 %
View Details
Ducoya® - G001 UP - Duvelco Limited
Duvelco Limited
Specs
Type Thermoplastic
Form / Shape Pellets
Chemical System Polyimide or Bismaleimide (BMI)
View Details
PEEK Polymer Resin - VICTREX® HT 22CA30 - Victrex PLC
Specs
Type ExtrusionGrade; MoldingCompound; Thermoplastic
Form / Shape Pellets
Chemical System PEEK
View Details
High Performance Polyimide Wire Enamels - ULTRATHERM - ELANTAS North America LLC
Specs
Type Thermally cured
Chemical System Polyimide or Bismaleimide (BMI)
Industry Electronics; Electrical Power or High Voltage
View Details