ASTM International Standard Test Methods for Chemical Analysis of Copper-Chromium Alloys ASTM E118-89(1996)

Description
1.1 These test methods cover procedures for the chemical analysis of chromium-copper alloys having chemical compositions within the following limits: Copper, % 98 and over Chromium, % 0.6 to 1.2 Silicon, % 0 to 0.10 Iron, % 0 to 0.10 1.2 The analytical procedures appear in the following order: Sections Copper by the Electrolytic Method 8 to 11 Chromium by the Dichromate (Potentiometric) Method 12 to 15 Silicon by the Perchloric Acid Dehydration Method 16
Request a Quote
Description
1.1 These test methods cover procedures for the chemical analysis of chromium-copper alloys having chemical compositions within the following limits: Copper, % 98 and over Chromium, % 0.6 to 1.2 Silicon, % 0 to 0.10 Iron, % 0 to 0.10 1.2 The analytical procedures appear in the following order: Sections Copper by the Electrolytic Method 8 to 11 Chromium by the Dichromate (Potentiometric) Method 12 to 15 Silicon by the Perchloric Acid Dehydration Method 16
Request a Quote

Suppliers

Company
Product
Description
Supplier Links
Standard Test Methods for Chemical Analysis of Copper-Chromium Alloys - ASTM E118-89(1996) - ASTM International
West Conshohocken, PA, United States
Standard Test Methods for Chemical Analysis of Copper-Chromium Alloys
ASTM E118-89(1996)
Standard Test Methods for Chemical Analysis of Copper-Chromium Alloys ASTM E118-89(1996)
1.1 These test methods cover procedures for the chemical analysis of chromium-copper alloys having chemical compositions within the following limits: Copper, % 98 and over Chromium, % 0.6 to 1.2 Silicon, % 0 to 0.10 Iron, % 0 to 0.10 1.2 The analytical procedures appear in the following order: Sections Copper by the Electrolytic Method 8 to 11 Chromium by the Dichromate (Potentiometric) Method 12 to 15 Silicon by the Perchloric Acid Dehydration Method 16

1.1 These test methods cover procedures for the chemical analysis of chromium-copper alloys having chemical compositions within the following limits:

Copper, % 98 and over Chromium, % 0.6 to 1.2 Silicon, % 0 to 0.10 Iron, % 0 to 0.10

1.2 The analytical procedures appear in the following order:

Sections Copper by the Electrolytic Method 8 to 11 Chromium by the Dichromate (Potentiometric) Method 12 to 15 Silicon by the Perchloric Acid Dehydration Method 16

Supplier's Site

Technical Specifications

  ASTM International
Product Category Standards and Technical Documents
Product Number ASTM E118-89(1996)
Product Name Standard Test Methods for Chemical Analysis of Copper-Chromium Alloys
Unlock Full Specs
to access all available technical data

Similar Products