ASTM International Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations ASTM D3217-95

Description
1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot. 1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included. 1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded. 1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Request a Quote
Description
1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot. 1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included. 1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded. 1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Request a Quote

Suppliers

Company
Product
Description
Supplier Links
Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations - ASTM D3217-95 - ASTM International
West Conshohocken, PA, United States
Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations
ASTM D3217-95
Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations ASTM D3217-95
1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot. 1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included. 1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded. 1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot.

1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included.

1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded.

1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Supplier's Site

Technical Specifications

  ASTM International
Product Category Standards and Technical Documents
Product Number ASTM D3217-95
Product Name Standard Test Methods for Breaking Tenacity of Manufactured Textile Fibers in Loop or Knot Configurations
Unlock Full Specs
to access all available technical data

Similar Products