ASTM International Standard Practice for Preparation of Low-Carbon Steel for Electroplating ASTM B183-79(2014)

Description
This practice provides an aid for setting up a suitable cleaning cycle preparatory to electroplating of low-carbon steel and indicates some of the precautions that must be taken to maintain this cycle in good operating condition. The preparatory procedure involves three basic steps in the following order: (1) removal of oils, grease, and caked-on dirt; (2) removal of scale and oxide films by pickling; and (3) removal of any smut left on the surface and activation of the steel. The cleaning of racked parts, which shall subsequently be electroplated in still tanks, agitated tanks, and semi- and full-automatic equipment, should be performed following this cycle: (1) precleaning; (2) electrocleaning; (3) water rinse; (4) acid pickling; (5) alkaline descaling; and (6) water rinse. Parts in bulk, which shall subsequently be electroplated in hand-operated or automatic barrels, should follow this cleaning cycle: (1) alkaline cleaning; (2) water rinse; (3) acid pickling; and (4) water rinse.
Request a Quote
Description
This practice provides an aid for setting up a suitable cleaning cycle preparatory to electroplating of low-carbon steel and indicates some of the precautions that must be taken to maintain this cycle in good operating condition. The preparatory procedure involves three basic steps in the following order: (1) removal of oils, grease, and caked-on dirt; (2) removal of scale and oxide films by pickling; and (3) removal of any smut left on the surface and activation of the steel. The cleaning of racked parts, which shall subsequently be electroplated in still tanks, agitated tanks, and semi- and full-automatic equipment, should be performed following this cycle: (1) precleaning; (2) electrocleaning; (3) water rinse; (4) acid pickling; (5) alkaline descaling; and (6) water rinse. Parts in bulk, which shall subsequently be electroplated in hand-operated or automatic barrels, should follow this cleaning cycle: (1) alkaline cleaning; (2) water rinse; (3) acid pickling; and (4) water rinse.
Request a Quote

Suppliers

Company
Product
Description
Supplier Links
Standard Practice for Preparation of Low-Carbon Steel for Electroplating - ASTM B183-79(2014) - ASTM International
West Conshohocken, PA, United States
Standard Practice for Preparation of Low-Carbon Steel for Electroplating
ASTM B183-79(2014)
Standard Practice for Preparation of Low-Carbon Steel for Electroplating ASTM B183-79(2014)
This practice provides an aid for setting up a suitable cleaning cycle preparatory to electroplating of low-carbon steel and indicates some of the precautions that must be taken to maintain this cycle in good operating condition. The preparatory procedure involves three basic steps in the following order: (1) removal of oils, grease, and caked-on dirt; (2) removal of scale and oxide films by pickling; and (3) removal of any smut left on the surface and activation of the steel. The cleaning of racked parts, which shall subsequently be electroplated in still tanks, agitated tanks, and semi- and full-automatic equipment, should be performed following this cycle: (1) precleaning; (2) electrocleaning; (3) water rinse; (4) acid pickling; (5) alkaline descaling; and (6) water rinse. Parts in bulk, which shall subsequently be electroplated in hand-operated or automatic barrels, should follow this cleaning cycle: (1) alkaline cleaning; (2) water rinse; (3) acid pickling; and (4) water rinse.

This practice provides an aid for setting up a suitable cleaning cycle preparatory to electroplating of low-carbon steel and indicates some of the precautions that must be taken to maintain this cycle in good operating condition. The preparatory procedure involves three basic steps in the following order: (1) removal of oils, grease, and caked-on dirt; (2) removal of scale and oxide films by pickling; and (3) removal of any smut left on the surface and activation of the steel. The cleaning of racked parts, which shall subsequently be electroplated in still tanks, agitated tanks, and semi- and full-automatic equipment, should be performed following this cycle: (1) precleaning; (2) electrocleaning; (3) water rinse; (4) acid pickling; (5) alkaline descaling; and (6) water rinse. Parts in bulk, which shall subsequently be electroplated in hand-operated or automatic barrels, should follow this cleaning cycle: (1) alkaline cleaning; (2) water rinse; (3) acid pickling; and (4) water rinse.

Supplier's Site

Technical Specifications

  ASTM International
Product Category Standards and Technical Documents
Product Number ASTM B183-79(2014)
Product Name Standard Practice for Preparation of Low-Carbon Steel for Electroplating
Unlock Full Specs
to access all available technical data

Similar Products